Tensile Yield Strength

SUBSTANCEVALUE
Structural steel ASTM A36 steel250 MPa
Steel, API 5L X65 (Fikret Mert Veral)448 MPa
Steel, high strength alloy ASTM A514690 MPa
Steel, prestressing strands1650 MPa
Stainless steel AISI 302 - Cold-rolled520 MPa
Cast iron 4.5% C, ASTM A-48130 MPa
Titanium alloy (6% Al, 4% V)830 MPa
Aluminium alloy 2014-T6[citation needed]400 MPa
Copper 99.9% Cu70 MPa
Cupronickel 10% Ni, 1.6% Fe, 1% Mn, balance Cu130 MPa
Silkworm silk500 MPa
Aramid (Kevlar or Twaron)3620 MPa
UHMWPE23 MPa
Bone (limb)45 MPa

Related